MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Diamond NYLON 66 Natural
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Nylon
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Linear Mold Shrinkage 0.013 cm/cm
@Thickness 3.17 mm
0.013 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 83.0 MPa12000 psiASTM D638
Elongation at Break 50 %50 %ASTM D882
Flexural Modulus 2.86 GPa415 ksiASTM D790
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
0.993 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 254 °C489 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hybrid Plastics MS0825 Nanoreinforced® POSS® Polyamide 6
BASF Ultramid® B24 NSD 05 PA6
Domo Domamid® 33 ABH Polyamide 6.6
Overview of materials for Nylon 66/6
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)

PDIAM445 / 126536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.