MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® CF 6 S PA*
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point.
  • Very high flexibility and toughness
  • Very good thermoforming and orientation properties
  • High shrink
  • Very good transparency
  • Low melting point (130°C)
Grilon CF 6 S is suitable for the manufacture of both flat and blown coextruded films with temperature sensitive polymers such as PVDC and EVOH. Typical applications are cook in bag for meat, cheese, deep-draw consumer and medical packaging and asymmetric barrier film structures.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³Dry; ISO 1183
Water Absorption 5.0 %5.0 %Sim. to ISO 62
Moisture Absorption 2.00 %2.00 %Sim. to ISO 62
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 180 g/10 min180 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 30.0 MPa4350 psiISO 527-3
Film Tensile Strength at Yield, TD 28.0 MPa4060 psiISO 527-3
Film Elongation at Break, MD 800 %800 %ISO 527-3
Film Elongation at Break, TD 900 %900 %ISO 527-3
Film Elongation at Yield, MD 15 %15 %ISO 527-3
Film Elongation at Yield, TD 8.0 %8.0 %ISO 527-3
Tensile Modulus 0.400 GPa58.0 ksiConditioned; ISO 527-1/-2
Tear Strength 65.0 kN/m371 pliTrouser Tear Resistance, Parallel; ISO 6383-1
 65.0 kN/m371 pliTrouser Tear Resistance, Normal; ISO 6383-1
Film Tensile Strength at Break, MD 85.0 MPa12300 psiISO 527-3
Film Tensile Strength at Break, TD 55.0 MPa7980 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °F10°C/min; ISO 11357-1/-3
 
Optical PropertiesMetricEnglishComments
Gloss 130 %130 %60°; ISO 2813
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)400ISO 15105-1/-2; 23°C/0% RH
 800ISO 15105-1/-2; 23°C/ 85% RH
Elmendorf Tear Resistance, Normal (N)80ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)80ISO 6383-2
EMS Gelboflextest [holes/m²]100
Food contactEU Requirements
FormGranules
Gelboflextest [holes/m²], EMS100
Oxygen Transmission Rate, cm³/(m²*d*bar)120ISO 15105-1/-2; 23°C/0% RH
 200ISO 15105-1/-2; 23°C/ 85% RH
PackagingOriented film
ProcessingBlown Film Extrusion
 Film Extrusion
 Other Extrusion
Product AttributesBarrier Properties
 Co Polyamide
 Flexible
 High viscosity
Special CharacteristicsTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamelt® 471 Copolyamide Hotmelt Adhesive
Techmer ES HiFill® PA6/12 CF30 BK 30% Carbon Filled
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced
Envalior Novamid® 3010CF30 BK PA66-CF30
EMS-Grivory Grilon® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45

PGRH224 / 156933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.