MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling LAMIGAMID® 600 Polyoxymethylene
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Application: friction bearings, wear and sliding liners

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: POM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³ISO R 1183
Moisture Absorption at Equilibrium 0.25 %0.25 %DIN 53473
Water Absorption at Saturation 0.60 %
@Temperature 20.0 °C
0.60 %
@Temperature 68.0 °F
ISO R 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 135 MPa19600 psiHc 30; ISO 2039; partially
Tensile Strength, Yield 68.0 MPa9860 psiISO-DIS 527
Creep Strength 13.0 MPa1890 psi1% elongation, 1000 h; DIN 53444
 22.0 MPa3190 psi2% elongation, 1000 h; DIN 53444
Tensile Modulus 3.50 GPa508 ksiDIN 53457
Flexural Strength 117 MPa17000 psiDIN 54352
Flexural Modulus 3.00 GPa435 ksiDIN 53457
Compressive Strength 50.0 MPa7250 psi5% pressing; EN ISO 604
 83.0 MPa12000 psi10% pressing; EN ISO 604
 103 MPa14900 psi20% pressing; EN ISO 604
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²DIN 53453
Izod Impact Resistance >= 9.00 J/cm²>= 42.8 ft-lb/in²swinging hammer 0,1 DIN 51222; DIN 53453
Coefficient of Friction 0.020 - 0.0800.020 - 0.080With lubrication
Coefficient of Friction, Dynamic 0.320.32no lube; Steel 2162, Rvst=2E-6m, p=0.05 Mpa, v=0.6 m/s, t=40°C
Tear Strength Test 0.600.60ISO-DIS 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN 53482
Surface Resistance 1.00e+13 ohm1.00e+13 ohmDIN 53482
Dielectric Constant 3.73.7DIN 53483
Dielectric Strength 70.0 kV/mm1780 kV/inDIN 53481
Dielectric Loss Index 0.00350.0035DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 100 µm/m-°C
@Temperature 20.0 - 100 °C
55.6 µin/in-°F
@Temperature 68.0 - 212 °F
DIN 53752
Specific Heat Capacity 1.46 J/g-°C0.349 BTU/lb-°F
Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FDIN 52612
Melting Point 167 °C333 °FISO R 1218
Maximum Service Temperature, Air 100 °C212 °FContinuous
 140 °C284 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FV-notch; ISO R 75
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FV-notch; ISO R 75
Minimum Service Temperature, Air -40.0 °C-40.0 °FContinuous
 
Descriptive Properties
Creepage/leakage ResistanceKA3bDIN 53480
Friction Wear0.9 micron/km

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient LubriOne™ ATH-000/04S Acetal (POM) Homopolymer
LATI Latilub 73/13-20T POM, PTFE Filled
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled

PSCHW028 / 90225

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.