MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Fibre Glast RAE 2426 / 2177 Epoxy  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Viscosity 680 cP680 cPASTM D2293
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989Cured; ASTM D2240
Tensile Strength at Break 275.0 MPa39880 psiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D638
Elongation at Break 1.87 %1.87 %Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D638
Tensile Modulus 16.8 GPa2440 ksiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.
Flexural Strength 374.69 MPa54344 psiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
Flexural Modulus 19.2 GPa2780 ksiProperty derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 62.8 °C145 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 60.0 min
@Temperature 25.0 °C
60.0 min
@Temperature 77.0 °F
4 fl. Oz.; ASTM D2471
 
Descriptive Properties
Mix Ratio100:21Resin:Hardener by Weight
 4:1Resin:Hardener by Volume

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fibre Glast Epolite 2427 Epoxy
Fibre Glast ProSet 125R / 229H Epoxy
Fibre Glast EZ Poxy EZ10 / EZ83 Epoxy
Solvay CYCOM® 5216 Epoxy - Unidirectional S-Glass Prepreg
Sumitomo Bakelite SUMILITE® ELC-4972R&S Glass Epoxy Laminate

PFIBRE14 / 38288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.