MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A.D. Compound Adene NCFA Homopolymer 20% CaCO3 Filled Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Calcium Carbonate (CaCO3) Filler

Material Notes: Information provided by A.D. Compound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Filler Content 20 %20 %ISO 3451 / 1
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ISO 868
Tensile Strength, Yield 25.0 MPa3630 psiISO 527
Elongation at Break 55 %55 %ISO 527
Elongation at Yield 8.5 %8.5 %ISO 527
Flexural Modulus 1.70 GPa247 ksiISO 178
Izod Impact, Notched (ISO) 3.80 kJ/m²1.81 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75
Vicat Softening Point 94.0 °C201 °F49 N; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A.D. Compound Adene NC180A Homopolymer 15% CaCO3 Filled Polypropylene
A.D. Compound Adene NCQA Homopolymer 40% CaCO3 Filled Polypropylene
A.D. Compound Adene NCWA Homopolymer 60% CaCO3 Filled Polypropylene
A.D. Compound Adene NCZA Homopolymer 70% CaCO3 Filled Polypropylene
A. Schulman ComAlloy Hiloy® 114 Polypropylene, Glass Reinforced, Chemically Coupled

PADCOM01 / 22579

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.