IDI Composites Dielectrite® 46-16 Thermoset Polyester, Molding
Categories:
Polymer
;
Thermoset
;
Polyester, TS
;
Thermoset Polyester Glass Filled BMC
Material Notes:
Premium high strength electrical grade with excellent resistance to smoke generation, weathering, and corrosive environments.
Data provided by IDI Composites.
Key Words:
BMC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.70
-
2.00
g/cc
0.0614
-
0.0723
lb/in³
Water Absorption
0.10 - 0.30 %
0.10 - 0.30 %
in 24 hours; ASTM D570
Mechanical Properties
Metric
English
Comments
Hardness, Barcol
30 - 60
30 - 60
ASTM D2583
Tensile Strength, Ultimate
55.0
MPa
7980
psi
ASTM D638
Tensile Modulus
12.0
GPa
1740
ksi
ASTM D638
Flexural Strength
124
MPa
18000
psi
ASTM D790
Flexural Modulus
12.0
GPa
1740
ksi
ASTM D790
Compressive Strength
179
MPa
26000
psi
ASTM D695
Izod Impact, Notched
7.47
J/cm
14.0
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Dielectric Strength
11.0
kV/mm
279
kV/in
ASTM D149
Arc Resistance
>=
180
sec
>=
180
sec
ASTM D495
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
>=
260
°C
>=
500
°F
ASTM D648
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Descriptive Properties
Bulk Factor App.
2.5
ASTM D1895
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
IDI Composites Dielectrite® 44-1 Thermoset Polyester, Molding
IDI Composites Dielectrite® 44-10 HGM Thermoset Polyester, Molding
IDI Composites Dielectrite® 44-10 MW Thermoset Polyester, Molding
IDI Composites Dielectrite® 44-10 Thermoset Polyester, Molding
IDI Composites Dielectrite® 46-09 Thermoset Polyester, Molding
PPTSB8 / 58279
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.