MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shinkong Synthetic Fibers Shinite® T102G15 PET, 15% Glass Filled, Fire Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced; Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes:

Information from Shinkong Synthetic Fibers Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
Water Absorption 0.15 %0.15 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm0.0060 - 0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 98.1 MPa14200 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Yield Strength 137 MPa19900 psiASTM D790
Flexural Modulus 6.08 GPa882 ksiASTM D790
Izod Impact, Notched 0.588 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.10 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.04.0ASTM D150
Dielectric Strength 20.0 kV/mm508 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shinkong Synthetic Fibers Shinite® D201M20 PBT, 20% Mineral Filled
Shinkong Synthetic Fibers Shinite® D201 PBT
Dow TORAY Z-6265 SILANE
Celanese Rynite® FR515 BK507 PET-GF15FR(17)
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant

PSHNK015 / 120785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.