MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® TPU™ Thermoplastic Polyurethane Honeycomb  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Designation: Material-Cell Size (inches)-Film Gauge (inches)-Outer Skin Thickness.
HexWeb® TPU™ is an attractive thermoplastic urethane honeycomb that has been developed using a proprietary fusing process. The core can be supplied either sandwiched between two face sheets of polyurethane material or stabilized by heat flanging the edges of the cells. The resulting HexWeb® TPU™ structure is eye-catching and flexible; it redirects energy, resists fatigue, and provides cushioning.
Specifications: Available in 7/32 inch, 9/32 inch, and 7/16 inch cell sizes. HexWeb® TPU™ core is available with a cell wall gauge of 0.012 inches.

Features: Energy redirection, Impact attenuation, Flexible, Cushioning, Lightweight, Durable, Visually appealing, Abrasion resistant, Tear and puncture resistant, Moisture resistant, Fatigue resistant, Complete recovery after impact (no permanent set), Amenable to wide temperature range, Thermally insulating.
Applications: HexWeb® TPU™ is an excellent material for any application requiring flexibility, cushioning, and withstanding repetitive impacts. This versatile honeycomb product is currently being used very successfully for energy redirection in soles of athletic footwear. It is also a superior product for use in interior cushions, body protection vests, orthopedic braces, and sports protective equipment. It has excellent fatigue resistance and remains flexible at low temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585Polyurethane material property, Hardness of Film; ASTM D2240
Taber Abrasion, mg/1000 Cycles 3030Polyurethane material property, 1000 gm load; ASTM C501
 
Thermal PropertiesMetricEnglishComments
Melting Point 171 - 193 °C340 - 380 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® DP 7-1158 Urethane Thermoplastic Elastomer
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU)
Barlog Plastics KEBAFLEX U A 75 ST B01 natural TPU, Shore A75, natural
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU

PHEXC420 / 98891

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.