MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced with this resin exhibit a unique low seal initiation temperature combined with high stiffness. Other features of this resin include good clarity and high machine direction tear resistance.

Applications/Uses

  • Food packaging
  • Trash bags
  • Blown film
  • Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Base Resin Density 0.917 g/cc0.0331 lb/in³ASTM D1505
    Thickness 25.0 microns0.984 milASTM D374
    Base Resin Melt Index 0.50 g/10 min0.50 g/10 minASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Film Tensile Strength at Yield, TD 9.00 MPa1310 psiASTM D882
    Film Elongation at Break, MD 600 %600 %ASTM D882
    Film Elongation at Break, TD 900 %900 %ASTM D882
    Elmendorf Tear Strength, MD 18.0 g/micron457 g/milASTM D1922
    Elmendorf Tear Strength, TD 28.0 g/micron711 g/milASTM D1922
    Dart Drop 30.0 g/micron762 g/milASTM D1709A
    Film Tensile Strength at Break, MD 59.0 MPa8560 psiASTM D882
    Film Tensile Strength at Break, TD 45.0 MPa6530 psiASTM D882
    1% Secant Modulus, MD 186 MPa27000 psiASTM D882
    1% Secant Modulus, TD 207 MPa30000 psiASTM D882
    Heat Seal Strength Initiation Temperature 96.0 °C205 °FEastman
     
    Optical PropertiesMetricEnglishComments
    Haze 18 %18 %ASTM D1003
    Gloss 50 %50 %at 45°; ASTM D2457
     
    Descriptive Properties
    ProcessFilm

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Westlake EC477AA Low Density Polyethylene
    Westlake EC476AA Low Density Polyethylene
    Westlake EC474AA Low Density Polyethylene
    Westlake EC472 Low Density Polyethylene
    Westlake EC471 Low Density Polyethylene

    PE9079 / 35135

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.