A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond strengths and outstanding chemical resistance. Requires elevate cure schedules. Information provided by Ellsworth Adhesives. |