MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

KKPC KOSYN KNB 35LL Acrylonitrile Butadiene Rubber (NBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Acrylonitrile Butadiene Rubber (NBR)

Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. Our NBR has superior working properties such as roll winding properties, compounding dispersibility and extrusion properties. Also, it is easily processed on account of the excellent vulcanization properties.

Applications: General oil-resistant Rubber Products such as packing, gasket, hose, rolls, and shoe soles

Additional Notes:
Bound Acrylonitrile: 34%
Compound Properties: NBR 100, ZnO 3, Stearic Acid 1, HAF Black (IRB#7) 40, Accelerator TBBS 1, Sulfur 1.5, Total: 146.5
Volume Change: -1%

This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.

Data provided by Korea Kumho Petrochemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Not Compounded
Mooney Viscosity  33
@Temperature 100 °C
33
@Temperature 212 °F
Raw; ML1+4
 58
@Temperature 100 °C
58
@Temperature 212 °F
Compounded; ML1+4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373150°C, 40 min., Pressure Vulcanization. 0% Change after 100°C, 70 hrs, Oil Immersion
Tensile Strength, Ultimate 29.4 MPa4270 psi150°C, 40 min., Pressure Vulcanization. -8% Change after 100°C, 70 hrs, Oil Immersion
Elongation at Break 590 %590 %150°C, 40 min., Pressure Vulcanization. -29% Change after 100°C, 70 hrs, Oil Immersion
300% Modulus 12.7 MPa
@Strain 300 %
1850 psi
@Strain 300 %
150°C, 40 min., Pressure Vulcanization. 42% Change after 100°C, 70 hrs, Oil Immersion
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.00 %
@Time 252000 sec
0.00 %
@Time 70.0 hour
after Oil Immersion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
ATG s.r.l. NBR Nitrile-Butadiene Rubber
Nitriflex NitriClean 3355 NBR - Nitrile Rubber
Metflex M52 NBR 50; Acrylonitrile butadiene rubber with low-medium CAN content
Armacell Ensolite™ IFC-400 Continuous Rolls/Sheets, PVC/NBR

PKKPC38 / 48769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.