MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vyncolit X655 Novolac Phenolic
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.

USES: Automotive disc brake pistons and gaskets, automatic gearbox thrust washers. Complex precision parts for compact disc players and automotive injection fuel pump bodies/impellers.

Information provided by Vyncolit, a Sumitomo Bakelite Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.05 g/cc0.0379 lb/in³Powder Density; ISO 60
Density 2.08 g/cc0.0751 lb/in³Relative Density; ISO 1183
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inInjection Molding; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiISO 527
Elongation at Break 0.40 %0.40 %Tensile; ISO 527
Tensile Modulus 28.0 GPa4060 ksiISO 527
Flexural Strength 170 MPa24700 psiAt Rupture; ISO 178
Flexural Modulus 25.0 GPa3630 ksiISO 178
Flexural Strain at Break 0.75 %0.75 %ISO 178
Compressive Strength 300 MPa43500 psiISO 604
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²ISO 179
Charpy Impact, Notched 0.250 J/cm²1.19 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+13 - 1.00e+14 ohm1.00e+13 - 1.00e+14 ohmDry; IEC 167
Dielectric Strength 30.0 kV/mm762 kV/inIEC 243
Comparative Tracking Index 200 V200 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature 20.0 °C
7.78 µin/in-°F
@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 20.0 µm/m-°C
@Temperature 20.0 °C
11.1 µin/in-°F
@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75 Af
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 4.00 mm
V-0
@Thickness 0.157 in
Shrinkage 0.010 %0.010 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorDark Green
ISO typePF 2 C3
Main FillerGlass Fiber & Mineral
Molding MethodCompression, transfer, injection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic
Sumitomo Bakelite North America RX® 655 Novolac Phenolic
Vyncolit X655/1 Glass Fiber and Mineral Filled Novolac Phenolic
BASF Procom® GC20H 250 Polypropylene
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend

PVYNC007 / 72215

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.