MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Cellulose Filled

Material Notes: RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-5948-96, Type CFI-5. (Replaces Military Specification MIL-M-14H.)

Information supplied by Sumitomo Bakelite North America.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 g/cc0.0145 lb/in³Powder; ASTM D1895
Density 1.43 g/cc0.0517 lb/in³ASTM D-792
Water Absorption 0.60 %0.60 %24 hour; ASTM D570
 1.5 %1.5 %48 hour; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7070ASTM D785
Tensile Strength, Ultimate 48.0 MPa6960 psiASTM D638
Flexural Strength 70.0 MPa10200 psiASTM D790
Flexural Modulus 10.0 GPa1450 ksiASTM D790
Compressive Strength 200 MPa29000 psiASTM D695
Izod Impact, Notched 0.600 J/cm1.12 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 3.40 kV/mm86.4 kV/in60 Hz, wet, SS; ASTM D149
 5.90 kV/mm150 kV/inST; ASTM D149
Arc Resistance 65 sec65 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 47.0 µm/m-°C
@Temperature 20.0 °C
26.1 µin/in-°F
@Temperature 68.0 °F
ASTM E831
CTE, linear, Transverse to Flow 53.0 µm/m-°C
@Temperature 20.0 °C
29.4 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Thermal Conductivity 0.560 W/m-K3.89 BTU-in/hr-ft²-°FASTM C518
Maximum Service Temperature, Air 150 °C302 °FUL Temperature Index; UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FAs Molded; ASTM D648A
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Descriptive Properties
Available Molding GradesCompression, Transfer, Injection
ColorBlack
FormPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate
Overview of materials for Phenolic, Novolac, Cellulose Filled

P90XR09 / 21223

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.