MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Fluorinert™ FC-3284 Electronic Liquid
Categories: Fluid

Material Notes: 3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package testing, power electronics and computer cooling.

Features and Benefits

  • Thermal stability
  • Chemical stability
  • Wide liquid range
  • Non-conductive
  • Narrow boiling range
  • Compatibility

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³Liquid
Viscosity 0.71 cP0.71 cPAbsolute
Kinematic Viscosity 0.42 cSt0.42 cSt
Molecular Weight 299 g/mol299 g/mol
Vapor Pressure 0.357 bar268 torr
 
Chemical PropertiesMetricEnglishComments
Critical Temperature 161 °C322 °FEstimated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 7.00e+15 ohm-cm7.00e+15 ohm-cm
Dielectric Constant 1.861.86
Dielectric Strength 1.57 kV/mm40.0 kV/in0.1" gap
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 105 J/g45.2 BTU/lbLatent, at normal boiling point
CTE, linear 1600 µm/m-°C889 µin/in-°F
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°FLiquid
Thermal Conductivity 0.0620 W/m-K0.430 BTU-in/hr-ft²-°FLiquid
Boiling Point 50.0 °C
@Pressure 0.101 MPa
122 °F
@Pressure 14.7 psi
Pour Point -73.0 °C-99.4 °F
 
Descriptive Properties
ColorClear, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Galden® HT70 PFPE Heat Transfer Fluid
3M Fluorinert™ FC-72 Electronic Liquid
3M Novec™ 612 Magnesium Protection Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 774 Engineered Fluid

PMM33090 / 167837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.