MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex HFFR 2006 Polyolefin, Halogen Free
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: RoHS Compliant

Features: Flame Retardant; Halogen Free

Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing

Agency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating

Processing Method: Extrusion

Forms: Pellets

Additional Information:

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 75%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 101%

Acid Gas, MIL-C-24643: < 5.0 mg

Acidity of Gases, IEC-754-2: < 6.0 pH

Conductivity: < 2.0 µS/cm

Smoke Index, NES-711: < 7.5

Toxicity Index, NES-713: 0.025

Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 430 kW/m2

Cone Calorimeter at 50 kW/m2, Total Heat Released: 140 MJ/m2

Cone Calorimeter at 50 kW/m2, Peak Smoke: 1.9 1/m

Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 91 sec

Information Provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D792
Melt Flow 7.6 g/10 min
@Load 10.0 kg,
Temperature 190 °C
7.6 g/10 min
@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 414110 seconds; ASTM D2240
Tensile Strength at Break 8.27 MPa1200 psiASTM D638
Elongation at Break 390 %390 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.10e+13 ohm-cm1.10e+13 ohm-cmASTM D257
Dielectric Constant 3.68
@Frequency 1000 Hz
3.68
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0067
@Frequency 1000 Hz
0.0067
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -28.0 °C-18.4 °FASTM D746
Oxygen Index 35 %35 %ASTM D2863
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyolefin, Wire/Cable Grade
AlphaGary Garaflex™ O 9949 RA Olefinic Thermoplastic Elastomer
Teknor Apex HFFR 2002 Polyolefin, Halogen Free
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled
Addiplast Addilene H 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled

PTEKNO599 / 128777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.