MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Thermx® LED 0201S PCT, 38% Specialty
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), Glass/Mineral Reinforced

Material Notes: Thermx LED 0201S is a super white reinforced PCT resin highly suitable for LED applications. The material exhibits high heat resistance, high reflectance stability, high thermal stability, low moisture absorption, and high mechanical properties for injection molding.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.0 %2.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 5.10 GPa740 ksi50mm/min; ISO 527-2/1A
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
Melting Point 285 °C545 °F10°C/min; ISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 150 °C212 - 302 °Fcavity
Zone 1 290 - 305 °C554 - 581 °F
Zone 2 285 - 300 °C545 - 572 °F
Zone 3 285 - 300 °C545 - 572 °F
Zone 4 285 - 300 °C545 - 572 °F
Die Temperature 285 - 295 °C545 - 563 °F
Melt Temperature 290 - 310 °C554 - 590 °F
Drying Temperature 95.0 - 100 °C203 - 212 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Thermx® TE3002 BK010 PCT
Eastman DuraStar DS1000 Polymer, Natural
Celanese Zenite® ZE16401 BK010 LCP
Celanese Zenite® 5145L WT010 LCP
Celanese Thermx® TE4004 PCT, 40% Specialty

PHCQ469 / 178924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.