MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Himod™ FT7324 LDPE for Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and improved optical properties. Benefits can be obtained in terms of better down gauging possibilities and improved processability. Excellent printing quality is obtained due to high clarity and better layout.

Himod FT7324 is intended for applications like: hygiene over-wrap films and co-extrusion applications.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.932 g/cc0.0337 lb/in³ISO 1183
Thickness 40.0 microns1.57 mil
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 550 ppm550 ppmAdditive - Synthetic Silica
Slip Level 750 ppm750 ppmAdditive - Erucamide
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 300 %300 %ISO 527-3
Film Elongation at Break, TD 500 %500 %ISO 527-3
Secant Modulus, MD 0.310 GPa45.0 ksiASTM D882-A
Secant Modulus, TD 0.360 GPa52.2 ksiASTM D882-A
Impact 2626Puncture Resistance, force (N); ASTM D5748
Puncture Energy 0.300 J0.221 ft-lbASTM D5748
Coefficient of Friction, Dynamic 0.200.20ISO 8295
Tear Strength, Total 2.50 N0.562 lb (f)TD; ISO 6383/2
 4.00 N0.899 lb (f)MD; ISO 6383/2
Dart Drop 2.00 g/micron50.8 g/milISO 7765/1
Film Tensile Strength at Break, MD 20.0 MPa2900 psiISO 527-3
Film Tensile Strength at Break, TD 15.0 MPa2180 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 118 °C244 °FISO 11357/03
Vicat Softening Point 107 °C225 °FA (10N); ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Himod™ FT7294 LDPE for Film
Borealis Himod™ FT3280 LDPE for Film
Borealis Himod™ FT5270 LDPE for Film
Borealis Himod™ FT6273 LDPE for Film
Borealis Himod™ FT6274 LDPE for Film

PBOREA179 / 27486

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.