MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Notes: Terraloy™ BP-20001A is a Thermoplastic Starch/Biodegradable Copolyester ready-to-process compound that contains up to 40% of TPS renewable content and is 100% biodegradable. This compound is for blown film applications as well as injection molded parts.

Processing Method: Blown Film; Injection Molding

Forms: Pellets

Additional Information: Biobased Content: < 40.0

Information Provided by Teknor Apex

Key Words: TPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Oxygen Transmission Rate 404 cc/m²/day26.0 cc/100 in²/dayASTM D1922
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 520 %520 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Elmendorf Tear Strength MD 300 g300 gASTM D1922
Elmendorf Tear Strength TD 380 g380 gASTM D1922
Dart Drop Test 290 g0.639 lbASTM D1709
Film Tensile Strength at Break, MD 26.0 MPa3770 psiASTM D882
Film Tensile Strength at Break, TD 20.3 MPa2940 psiASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Biomax® TPS 2100
BiologiQ EcoStarch GS270 Thermoplastic Starch
Teknor Apex Terraloy™ MB 20001A Thermoplastic Starch + Copolyester
DuPont Biomax® TPS 2501
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE

PTEKNO812 / 128993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.