MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultrason® E 2010 PES
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA requirements of 21 CFR 177.2440.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Water Absorption 2.2 %2.2 %ISO 62
Moisture Absorption at Equilibrium 0.80 %0.80 %23°C/50% R.H.; ISO 62
Viscosity Number 56 cm³/g0.56 dl/g
Linear Mold Shrinkage, Flow 0.0082 cm/cm0.0082 in/inISO 294
Linear Mold Shrinkage, Transverse 0.0086 cm/cm0.0086 in/inISO 294
Melt Flow 70 g/10 min
@Load 10.0 kg,
Temperature 360 °C
70 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 154 MPa22300 psiISO 2039-1
Tensile Strength at Break 90.0 MPa13100 psi5mm/min; ISO 527-2
Tensile Strength, Yield 90.0 MPa13100 psi50mm/min; ISO 527-2
Elongation at Break 6.7 %6.7 %5mm/min; ISO 527-2
Elongation at Yield 6.7 %6.7 %50mm/min; ISO 527-2
Modulus of Elasticity 2.50 GPa
@Temperature 60.0 °C
363 ksi
@Temperature 140 °F
ISO 527
Tensile Modulus 2.70 GPa392 ksiISO 527-2
Flexural Strength 131 MPa19000 psiISO Data
Flexural Modulus 2.60 GPa377 ksiASTM Test
 2.86 GPa415 ksiISO Data
Fatigue Strength  5.00 MPa
@# of Cycles 1.00e+7 ,
Temperature 180 °C
725 psi
@# of Cycles 1.00e+7 ,
Temperature 356 °F
 7.00 MPa
@# of Cycles 1.00e+6 ,
Temperature 180 °C
1020 psi
@# of Cycles 1.00e+6 ,
Temperature 356 °F
 9.00 MPa
@# of Cycles 100000 ,
Temperature 180 °C
1310 psi
@# of Cycles 100000 ,
Temperature 356 °F
 12.0 MPa
@# of Cycles 10000 ,
Temperature 180 °C
1740 psi
@# of Cycles 10000 ,
Temperature 356 °F
 22.0 MPa
@# of Cycles 1.00e+7
3190 psi
@# of Cycles 1.00e+7
 25.0 MPa
@# of Cycles 100000
3630 psi
@# of Cycles 100000
 35.0 MPa
@# of Cycles 100000
5080 psi
@# of Cycles 100000
 55.0 MPa
@# of Cycles 10000
7980 psi
@# of Cycles 10000
Shear Modulus  0.200 GPa
@Temperature 225 °C
29.0 ksi
@Temperature 437 °F
ISO 6721
 0.900 GPa
@Temperature 200 °C
131 ksi
@Temperature 392 °F
ISO 6721
 0.950 GPa
@Temperature 100 °C
138 ksi
@Temperature 212 °F
ISO 6721
 1.00 GPa
@Temperature 50.0 °C
145 ksi
@Temperature 122 °F
ISO 6721
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO 180/A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²3.09 ft-lb/in²ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 2700 MPa392000 psielongation <0.5%, 23°C; ISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm940 kV/inIEC 60243-1
Dissipation Factor  0.0017
@Frequency 100 Hz
0.0017
@Frequency 100 Hz
IEC 60250
 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VTest Liquid A & B; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear  50.0 µm/m-°C
@Temperature -26.0 °C
27.8 µin/in-°F
@Temperature -14.8 °F
DIN 53752
 54.0 µm/m-°C
@Temperature 75.0 °C
30.0 µin/in-°F
@Temperature 167 °F
DIN 53752
 60.0 µm/m-°C
@Temperature 175 °C
33.3 µin/in-°F
@Temperature 347 °F
DIN 53752
CTE, linear, Parallel to Flow 52.0 µm/m-°C28.9 µin/in-°FISO 11359-1/-2
 59.0 µm/m-°C32.8 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 220 °C428 °F
Deflection Temperature at 0.46 MPa (66 psi) 218 °C424 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-2
Glass Transition Temp, Tg 225 °C437 °FISO 11357-1/-3
UL RTI, Electrical 190 °C374 °F50% decrease of tensile strength after 20000h; 746B
Flammability, UL94  V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
Oxygen Index 38 %38 %ISO 4589-1/-2
Glow Wire Ignition Temperature 825 °C1520 °FIEC 60695-2-13
Glow Wire Flammability Index 960 °C1760 °FIEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.651.65
Transmission, Visible 88 %
@Thickness 50.8 mm
88 %
@Thickness 2.00 in
ASTM D 1003
 30 %
@Wavelength 350 nm
30 %
@Wavelength 350 nm
 72 %
@Wavelength 400 nm
72 %
@Wavelength 400 nm
 81 %
@Wavelength 500 nm
81 %
@Wavelength 500 nm
 85 %
@Wavelength 600 nm
85 %
@Wavelength 600 nm
UV Transmittance  2.0 %
@Wavelength 300 nm
2.0 %
@Wavelength 300 nm
 15 %
@Wavelength 200 nm
15 %
@Wavelength 200 nm
 
Processing PropertiesMetricEnglishComments
Melt Temperature 340 - 390 °C644 - 734 °FInjection molding
Mold Temperature 140 - 180 °C284 - 356 °FInjection molding
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.2440
NSF YesYesNSF Std. 51
 YesYesNSF Std. 61
 
Descriptive Properties
ColorNatural and colored
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding, Extrusion, and Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® E 3010 PES
BASF Ultrason® E 1010 PES
Aclo Accucomp ABS ABS802L High Impact Grade
BASF Ultrason® E 2010 G6 30% Glass Filled PES
Colorite Polymers 4011G-015 (Extrustion), 4012G-015 (Molding) Radiation Sterilizable Vinyl Compound

PBASF9399 / 85163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.