MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 3378A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion grade; Hoses, non-reinforced

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ISO 868
Tensile Strength, Ultimate 43.0 MPa6240 psi200 mm/min; DIN 53504
Elongation at Break 684 %684 %200 mm/min; DIN 53504
Tensile Modulus  0.0120 GPa
@Temperature 60.0 °C
1.74 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0220 GPa
@Temperature 20.0 °C
3.19 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.0460 GPa
@Temperature -20.0 °C
6.67 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
100% Modulus 3.90 MPa
@Strain 100 %
566 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 9.70 MPa
@Strain 200 %
1410 psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound 57 %57 %Resilience; ISO 4662
Tear Strength 67.0 kN/m382 pli500 mm/min; ISO 34-1
Abrasion 3131mm3; ISO 4649 method A
Compression Set  9.0 %
@Temperature 70.0 °C,
Time 86400 sec
9.0 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method C
 16 %
@Temperature 70.0 °C,
Time 86400 sec
16 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 46 %
@Temperature 23.0 °C,
Time 259000 sec
46 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 220 °C392 - 428 °FExtrusion
 210 - 230 °C410 - 446 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 90.0 °C194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 2786A GMP TPU
Covestro Desmopan® 3360A DPS 061 TPU
Covestro Desmopan® 2786A GMP 045 TPU
Covestro Desmopan® 9370A GMP TPU
Covestro Desmopan® 9864DU TPU

PCOVEST0706 / 202489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.