MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Crastin® 6131 NC010 PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Unreinforced Low Viscosity Polybutylene Terephthalate

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Melt Density 1.11 g/cc
@Temperature >=225 °C
0.0401 lb/in³
@Temperature >=437 °F
Water Absorption 0.40 %
@Thickness 2.00 mm
0.40 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Viscosity Number 110 cm³/g1.10 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.016 cm/cm0.016 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4, 2577
Melt Flow 48 g/10 min
@Load 2.16 kg,
Temperature 250 °C
48 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 59.0 MPa8560 psiISO 527-1/-2
Elongation at Break 30 %30 %Nominal; ISO 527-1/-2
Elongation at Yield 6.0 %6.0 %ISO 527-1/-2
Tensile Modulus 2.60 GPa377 ksiISO 527-1/-2
Flexural Strength 85.0 MPa12300 psiISO 178
Poissons Ratio 0.380.38ISO 527-1/-2
Izod Impact, Notched (ISO) 3.50 kJ/m²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 62631-3-2
Dielectric Strength 26.0 kV/mm660 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 108 µm/m-°C60.0 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 144 µm/m-°C80.0 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 2.05 J/g-°C
@Temperature >=225 °C
0.490 BTU/lb-°F
@Temperature >=437 °F
Melt
Thermal Conductivity 0.250 W/m-K
@Temperature >=225 °C
1.74 BTU-in/hr-ft²-°F
@Temperature >=437 °F
Melt
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FISO 75-1/-2
 180 °C356 °FAnnealed; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FISO 75-1/-2
 60.0 °C140 °FAnnealed; ISO 75-1/-2
Vicat Softening Point 175 °C347 °F50°C/h, 50N; ISO 306
Flammability, UL94  HB
@Thickness 0.880 mm
HB
@Thickness 0.0346 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 22 %22 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 °C482 °FInjection Optimum
 240 - 260 °C464 - 500 °FInjection
Mold Temperature 80.0 °C176 °FInjection Optimum
 30.0 - 130 °C86.0 - 266 °FInjection
Ejection Temperature 170 °C338 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer
Moisture Content 0.040 %0.040 %
Hold Pressure 60.0 MPa8700 psi
 
Descriptive Properties
Back pressureAs low as possible
Delivery formPellets
Drying Recommendedyes
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)4
Part Marking CodePBTISO 11469
ProcessingCasting
 Coatable
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Regional AvailabilityEurope
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPBTISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Crastin® 6134 NC010 PBT
DuPont Mobility and Materials Crastin® 6130 NC010 PBT
DuPont Mobility and Materials Crastin® 6129 NC010 PBT
Celanese Crastin® S600F10 BK851 PBT
Intercontinental Polymers 553 PBT Polymer Type - Elastomer, Polyester Pellets

PDSX5002 / 197642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.