MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 6, 40% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.35 - 2.01 g/cc0.0488 - 0.0724 lb/in³Average value: 1.49 g/cc Grade Count:93
 1.28 - 1.291 g/cc
@Temperature 220 - 270 °C
0.0462 - 0.04664 lb/in³
@Temperature 428 - 518 °F
Average value: 1.29 g/cc Grade Count:6
Filler Content 35.0 - 40.0 %35.0 - 40.0 %Average value: 39.6 % Grade Count:18
Water Absorption 0.700 - 6.00 %0.700 - 6.00 %Average value: 2.07 % Grade Count:55
Moisture Absorption at Equilibrium 0.250 - 2.30 %0.250 - 2.30 %Average value: 1.66 % Grade Count:34
Water Absorption at Saturation 3.40 - 7.00 %3.40 - 7.00 %Average value: 5.20 % Grade Count:20
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm0.00100 - 0.0180 in/inAverage value: 0.00779 cm/cm Grade Count:72
Linear Mold Shrinkage, Transverse 0.00300 - 0.0140 cm/cm0.00300 - 0.0140 in/inAverage value: 0.00886 cm/cm Grade Count:30
Melt Flow 3.00 - 33.0 g/10 min3.00 - 33.0 g/10 minAverage value: 19.0 g/10 min Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 81.0 - 12281.0 - 122Average value: 110 Grade Count:11
Hardness, Rockwell R 103 - 122103 - 122Average value: 119 Grade Count:18
 25.0 - 30.0
@Temperature 80.0 - 80.0 °C
25.0 - 30.0
@Temperature 176 - 176 °F
Average value: 27.5 Grade Count:1
Ball Indentation Hardness 85.0 - 260 MPa12300 - 37700 psiAverage value: 175 MPa Grade Count:10
Tensile Strength, Ultimate 35.0 - 207 MPa5080 - 30000 psiAverage value: 81.3 MPa Grade Count:74
 20.0 - 135 MPa
@Temperature -40.0 - 150 °C
2900 - 19600 psi
@Temperature -40.0 - 302 °F
Average value: 61.9 MPa Grade Count:9
Tensile Strength, Yield 45.0 - 114 MPa6530 - 16500 psiAverage value: 81.4 MPa Grade Count:27
 20.0 - 90.0 MPa
@Temperature -40.0 - 120 °C
2900 - 13100 psi
@Temperature -40.0 - 248 °F
Average value: 45.0 MPa Grade Count:1
Elongation at Break 1.50 - 40.0 %1.50 - 40.0 %Average value: 11.8 % Grade Count:80
 2.00 - 60.0 %
@Temperature -40.0 - 150 °C
2.00 - 60.0 %
@Temperature -40.0 - 302 °F
Average value: 25.9 % Grade Count:5
Elongation at Yield 2.50 - 27.0 %2.50 - 27.0 %Average value: 7.84 % Grade Count:16
 5.10 - 30.0 %
@Temperature -40.0 - 120 °C
5.10 - 30.0 %
@Temperature -40.0 - 248 °F
Average value: 20.0 % Grade Count:1
Modulus of Elasticity 2.00 - 12.8 GPa290 - 1860 ksiAverage value: 5.42 GPa Grade Count:48
 0.600 - 8.31 GPa
@Temperature -40.0 - 150 °C
87.0 - 1210 ksi
@Temperature -40.0 - 302 °F
Average value: 3.12 GPa Grade Count:5
Flexural Yield Strength 50.0 - 290 MPa7250 - 42100 psiAverage value: 120 MPa Grade Count:78
 25.0 - 207 MPa
@Temperature -40.0 - 120 °C
3630 - 30000 psi
@Temperature -40.0 - 248 °F
Average value: 86.2 MPa Grade Count:7
Flexural Modulus 1.50 - 10.7 GPa218 - 1550 ksiAverage value: 5.42 GPa Grade Count:84
 0.700 - 8.60 GPa
@Temperature -40.0 - 120 °C
102 - 1250 ksi
@Temperature -40.0 - 248 °F
Average value: 2.88 GPa Grade Count:8
Flexural Strain at Break 2.00 - 9.00 %2.00 - 9.00 %Average value: 5.77 % Grade Count:11
Compressive Yield Strength 69.0 - 186 MPa10000 - 27000 psiAverage value: 129 MPa Grade Count:4
Poissons Ratio 0.350 - 0.3900.350 - 0.390Average value: 0.360 Grade Count:3
Izod Impact, Notched 0.267 - 100 J/cm0.500 - 187 ft-lb/inAverage value: 0.663 J/cm Grade Count:38
 0.320 - 0.820 J/cm
@Temperature -40.0 - -40.0 °C
0.599 - 1.54 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.578 J/cm Grade Count:3
Izod Impact, Unnotched 0.374 - 16.4 J/cm0.700 - 30.7 ft-lb/inAverage value: 5.75 J/cm Grade Count:9
Izod Impact, Notched (ISO) 3.00 - 11.0 kJ/m²1.43 - 5.23 ft-lb/in²Average value: 7.77 kJ/m² Grade Count:31
 4.00 - 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
1.90 - 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 9.04 kJ/m² Grade Count:11
Izod Impact, Unnotched (ISO) 25.0 kJ/m² - NB11.9 ft-lb/in² - NBAverage value: 77.8 kJ/m² Grade Count:13
 25.0 - 100 kJ/m²
@Temperature -30.0 - -30.0 °C
11.9 - 47.6 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 69.5 kJ/m² Grade Count:10
Charpy Impact Unnotched 0.300 J/cm² - NB1.43 ft-lb/in² - NBAverage value: 7.90 J/cm² Grade Count:35
 1.80 J/cm² - NB
@Temperature -40.0 - -20.0 °C
8.57 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 6.21 J/cm² Grade Count:21
Charpy Impact, Notched 0.200 - 1.20 J/cm²0.952 - 5.71 ft-lb/in²Average value: 0.691 J/cm² Grade Count:52
 0.200 - 1.00 J/cm²
@Temperature -40.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.778 J/cm² Grade Count:21
Puncture Energy 9.20 - 65.0 J6.79 - 47.9 ft-lbAverage value: 37.7 J Grade Count:6
 1.60 - 3.00 J
@Temperature -30.0 - -30.0 °C
1.18 - 2.21 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 2.72 J Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 - 1.00e+16 ohm-cm1.00e+9 - 1.00e+16 ohm-cmAverage value: 3.91e+14 ohm-cm Grade Count:34
Surface Resistance 1.00e+10 - 7.00e+15 ohm1.00e+10 - 7.00e+15 ohmAverage value: 7.10e+14 ohm Grade Count:13
Dielectric Constant 3.60 - 15.03.60 - 15.0Average value: 5.46 Grade Count:14
Dielectric Strength 16.0 - 42.1 kV/mm406 - 1070 kV/inAverage value: 27.6 kV/mm Grade Count:24
Dissipation Factor 0.0100 - 0.2500.0100 - 0.250Average value: 0.0586 Grade Count:13
Arc Resistance 120 - 190 sec120 - 190 secAverage value: 140 sec Grade Count:6
Comparative Tracking Index 400 - 600 V400 - 600 VAverage value: 528 V Grade Count:16
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.20 - 103 µm/m-°C4.00 - 57.0 µin/in-°FAverage value: 52.7 µm/m-°C Grade Count:33
CTE, linear, Transverse to Flow 30.0 - 75.0 µm/m-°C16.7 - 41.7 µin/in-°FAverage value: 61.8 µm/m-°C Grade Count:11
Specific Heat Capacity 2.00 - 2.00 J/g-°C0.478 - 0.478 BTU/lb-°FAverage value: 2.00 J/g-°C Grade Count:5
 1.94 - 1.94 J/g-°C
@Temperature 270 - 270 °C
0.464 - 0.464 BTU/lb-°F
@Temperature 518 - 518 °F
Average value: 1.94 J/g-°C Grade Count:1
Thermal Conductivity 0.281 - 1.30 W/m-K1.95 - 9.02 BTU-in/hr-ft²-°FAverage value: 0.616 W/m-K Grade Count:7
 0.270 - 0.270 W/m-K
@Temperature 270 - 270 °C
1.87 - 1.87 BTU-in/hr-ft²-°F
@Temperature 518 - 518 °F
Average value: 0.270 W/m-K Grade Count:1
Melting Point 215 - 325 °C419 - 617 °FAverage value: 226 °C Grade Count:51
Maximum Service Temperature, Air 65.0 - 270 °C149 - 518 °FAverage value: 123 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 130 - 290 °C266 - 554 °FAverage value: 198 °C Grade Count:42
Deflection Temperature at 1.8 MPa (264 psi) 79.4 - 240 °C175 - 464 °FAverage value: 135 °C Grade Count:69
Deflection Temperature at 8.0 MPa 50.0 - 115 °C122 - 239 °FAverage value: 70.0 °C Grade Count:5
Vicat Softening Point 175 - 230 °C347 - 446 °FAverage value: 207 °C Grade Count:17
Flammability, UL94 HB - V-0HB - V-0Grade Count:41
Oxygen Index 24.0 - 30.0 %24.0 - 30.0 %Average value: 26.6 % Grade Count:7
Glow Wire Test 650 - 750 °C1200 - 1380 °FAverage value: 663 °C Grade Count:10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 221 - 290 °C430 - 554 °FAverage value: 265 °C Grade Count:7
Nozzle Temperature 250 - 293 °C482 - 560 °FAverage value: 268 °C Grade Count:6
Melt Temperature 230 - 300 °C446 - 572 °FAverage value: 272 °C Grade Count:41
Mold Temperature 43.0 - 121 °C109 - 250 °FAverage value: 87.4 °C Grade Count:48
Drying Temperature 73.9 - 180 °C165 - 356 °FAverage value: 88.7 °C Grade Count:17
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.140 % Grade Count:11
Injection Pressure 3.45 - 138 MPa500 - 20000 psiAverage value: 49.8 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Mineral Filled
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
Overview of materials for Nylon 6, 20% Mineral Filled
Overview of materials for Nylon 6, Glass/Mineral Reinforced
Overview of materials for Nylon 66/6, Mineral Reinforced

O2424 / 77984

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.