MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: Features:
  • High dielectric constant for circuit size reduction
  • Low loss - Ideal for operating at X-band or below
  • Low Z-axis expansion. Provides reliable plated through holes in multi-layer boards
  • Tight dielectric constant and thickness control for repeatable circuit performance
  • Cladding - EDC or rolled copper foil, also thick aluminum, brass or copper plate (one side)
  • Lead-free process compatible

Typical Applications:

  • Space Saving Circuitry
  • Patch Antennas
  • Ground Radar Warning Systems
  • Satellite Communications Systems
  • Power Amplifiers
  • Aircraft Collision Avoidance Systems

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.10 g/cc0.112 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.010 %
@Temperature 50.0 °C,
Time 173000 sec
0.010 %
@Temperature 122 °F,
Time 48.0 hour
0.05 in.; IPC-TM-650 2.6.2.1
Thickness 127 - 2540 microns5.00 - 100 milRange of Standard Thicknesses
Deformation  0.26 %
@Pressure 7.00 MPa,
Temperature 50.0 °C
0.26 %
@Pressure 1020 psi,
Temperature 122 °F
Z direction; 24 hrs; ASTM D621
 1.37 %
@Pressure 7.00 MPa,
Temperature 150 °C
1.37 %
@Pressure 1020 psi,
Temperature 302 °F
Z direction; 24 hrs; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 13.0 MPa1890 psiY direction; 0.1/min strain rate; ASTM D638
 17.0 MPa2470 psiX direction; 0.1/min strain rate; ASTM D638
Elongation at Break 7.0 - 14 %7.0 - 14 %Y direction; 0.1/min strain rate; ASTM D638
 9.0 - 15 %9.0 - 15 %X direction; 0.1/min strain rate; ASTM D638
Flexural Strength 32.0 MPa4640 psiY direction, Condition A; ASTM D790
 36.0 MPa5220 psiX direction, Condition A; ASTM D790
Flexural Modulus 3.751 GPa544.0 ksiY direction, Condition A; ASTM D790
 4.364 GPa632.9 ksiX direction, Condition A; ASTM D790
Compressive Yield Strength 47.0 MPa
@Strain 25 %
6820 psi
@Strain 25 %
Z direction; 0.05/min strain rate; ASTM D695
Compressive Modulus 2.144 GPa311.0 ksiZ direction; 0.05/min strain rate; ASTM D695
Peel Strength 2.16 kN/m12.3 pliCopper, after solder float; IPC-TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+12 ohm-cm5.00e+12 ohm-cmCondition A; IPC 2.5.17.1
Surface Resistance 5.00e+12 ohm5.00e+12 ohmCondition A; IPC 2.5.17.1
Dielectric Constant  9.95 - 10.45
@Frequency 1e+10 Hz
9.95 - 10.45
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 10.9
@Frequency 8.00e+9 - 4.00e+10 Hz
10.9
@Frequency 8.00e+9 - 4.00e+10 Hz
Differential Phase Length Method
Dissipation Factor 0.0023
@Frequency 1e+10 Hz
0.0023
@Frequency 1e+10 Hz
Z direction; IPC-TM-650 2.5.5.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear  24.0 µm/m-°C
@Temperature 0.000 - 100 °C
13.3 µin/in-°F
@Temperature 32.0 - 212 °F
X-Direction; 5°C/min; ASTM D3386
 24.0 µm/m-°C
@Temperature 0.000 - 100 °C
13.3 µin/in-°F
@Temperature 32.0 - 212 °F
Y-Direction; 5°C/min; ASTM D3386
 47.0 µm/m-°C
@Temperature 0.000 - 100 °C
26.1 µin/in-°F
@Temperature 32.0 - 212 °F
Z-Direction; 5°C/min; ASTM D3386
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°Fcalculated
Thermal Conductivity 0.860 W/m-K
@Temperature 80.0 °C
5.97 BTU-in/hr-ft²-°F
@Temperature 176 °F
ASTM C518
Decomposition Temperature 500 °C932 °FTGA; ASTM D3850
Flammability, UL94 V-0V-0
 
Descriptive Properties
Thermal Coefficient of Dielectric Constant-425 ppm/°CIPC-TM-650 2.5.5.5; 10 GHz; -50°C to 170°C; Z-Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
Copper, Cu; Annealed
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
Copper, Cu; Cold Drawn
AGC Fluon® FC123 PTFE, 15% Graphite Filled

PROGA975 / 138415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.