Flint Hills AP6835-HS Polypropylene Impact Copolymer
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene Copolymer
;
Polypropylene, Impact Modified; Molded/Extruded
Material Notes:
Features:
Excellent processing, good low temperature impact strength.
Applications:
Injection molding: Appliance components, consumer durables and closures
Information Provided by Flint Hills Resources
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.900
g/cc
0.0325
lb/in³
ASTM D1505
Melt Flow
35
g/10 min
35
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
91
91
ASTM D785
Tensile Strength, Yield
21.0
MPa
3050
psi
ASTM D638
Izod Impact, Notched
1.53
J/cm
@Temperature 23.0 °C
2.87
ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact
36.0
J
@Temperature -30.0 °C
26.6
ft-lb
@Temperature -22.0 °F
ASTM D5420
Tangent Modulus
1104
MPa
160100
psi
ASTM D790
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
85.0
°C
185
°F
ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Flint Hills AP4135-HS Polypropylene Impact Copolymer
Flint Hills AP5135-HS Impact Copolymer Polypropylene
Flint Hills AP7535-HS Polypropylene Ultra High Impact Copolymer
Flint Hills P6C6B-134 General Purpose Impact Copolymer Polypropylene
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene
PFLINT017 / 104571
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.