MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Polystone® G Pipe Grade HDPE/PE300
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
  • Excellent weldability
  • UV-stabilized and colorfast
  • Good chemical resistance
Product applications:
  • Stub ends
  • Flanges & fittings
  • Manhole bases & covers

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D792
Water Absorption <= 0.10 %<= 0.10 %ASTM D570
Carbon Black Loading 2.0 %2.0 %ISO 6964
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 24.99 MPa3625 psiASTM D638
Elongation at Break >= 600 %>= 600 %ASTM D638
Tensile Modulus 1.03 GPa150 ksiASTM D638
Flexural Modulus 0.827 GPa120 ksiASTM D790
 1.03 GPa150 ksiASTM D790
Izod Impact, Notched 4.81 J/cm9.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 108 µm/m-°C60.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 82.2 °C180 °F
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °FASTM D648
Vicat Softening Point 126 °C259 °FISO 306
Brittleness Temperature -118 °C-180 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
NSF NoNo
USDA NoNo
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polimersan Plastics POLIPOLEN® (Polyethylene) HD-PE 300
Isoflon PEHD 500 High Density Polyethylene
Versalis Eraclene® MR 80 High Density Polyethylene - Injection Molding
Vapla Vaplatec 500 High Molecular Weight Polyethylene
Vapla Vaplatec 1000 Ultra High Molecular Weight Polyethylene

PROCH9016 / 232720

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.