MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow D 114.01 Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Developmental Performance Polymer

Information provided by Dow

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.903 g/cc0.0326 lb/in³ISO 1183
Linear Mold Shrinkage 0.017 cm/cm0.017 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0194 cm/cm0.0194 in/inISO 2577
Melt Flow 0.42 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.42 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.3 MPa2220 psi50mm/min; ISO R527
Tensile Strength, Yield 29.4 MPa4260 psi50mm/min; ISO R527
Elongation at Break 23 %23 %50mm/min; ISO R527
Elongation at Yield 8.1 %8.1 %50mm/min; ISO R527
Modulus of Elasticity 1.383 GPa200.6 ksi50mm/min; ISO R527
Flexural Strength 34.0 MPa4930 psiISO 178
Flexural Modulus 1.508 GPa218.7 ksi2 mm/min; ISO 178
Poissons Ratio 0.430.431 mm/min; ISO 527
Shear Modulus 0.469 GPa68.0 ksiISO 6721-6
Izod Impact, Notched (ISO) 35.7 kJ/m²17.0 ft-lb/in²ISO 180/1A
 5.25 kJ/m²
@Temperature -40.0 °C
2.50 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
Charpy Impact, Notched 48.2 J/cm²229 ft-lb/in²ISO 179/1A
 3.40 J/cm²
@Temperature -40.0 °C
16.2 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 114.5 µm/m-°C
@Temperature -30.0 - 100 °C
63.61 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D696
CTE, linear, Transverse to Flow 153.2 µm/m-°C
@Temperature -30.0 - 100 °C
85.11 µin/in-°F
@Temperature -22.0 - 212 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 90.8 °C195 °FFlatwise; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 52.3 °C126 °FFlatwise; ISO 75
Flame Spread 18 mm/min0.71 in/minFMVSS 302

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene, Molded
Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Flint Hills P4G4Z-011 Homopolymer Polypropylene
316 Stainless Steel, annealed sheet

PDOW1133 / 30337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.