MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

303 Stainless Steel, cold drawn bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Key Words: T303, T 303, 303SS, 303 SS, AFNOR Z 10 CNF 18.09 (Fr), UNI X 10 CrNiS 18 09, SUS 303, SS14 2346 (Sweden), B.S. 303 S 21, UNS S30300, AMS 5640 (1), ASME SA194, ASME SA320, ASTM A194, ASTM A314, ASTM A320, ASTM A320, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (30303), DIN 1.4305, X12CrNiS188, EN 58M, austenitic, ISO 683/13 17, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 228228
Hardness, Knoop 251251Converted from Brinell
Hardness, Rockwell B 9696Converted from Brinell
Hardness, Rockwell C 1919Converted from Brinell hardness. Value below normal HRC range, for comparison only.
Hardness, Vickers 240240Converted from Brinell
Tensile Strength, Ultimate 690 MPa100000 psi
Tensile Strength, Yield 415 MPa
@Strain 0.2 %
60200 psi
@Strain 0.2 %
Elongation at Break 40 %40 %in 50 mm
Tensile Modulus 193 GPa28000 ksi
Poissons Ratio 0.250.25Calculated
Fatigue Strength 240 MPa34800 psiannealed sample
 330 MPa47900 psi25% hardened sample
Shear Modulus 77.2 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.2 µm/m-°C
@Temperature 0.000 - 100 °C
9.56 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
9.89 µin/in-°F
@Temperature 32.0 - 599 °F
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
10.2 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.2 W/m-K
@Temperature 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.5 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1420 °C2550 - 2590 °F
Solidus 1400 °C2550 °F
Liquidus 1420 °C2590 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 18 %18 %
Iron, Fe 69 %69 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.60 %<= 0.60 %
Nickel, Ni 9.0 %9.0 %
Phosphorus, P <= 0.20 %<= 0.20 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S >= 0.15 %>= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed bar
303 Stainless Steel, annealed
304 Stainless Steel
303 SE Stainless Steel, cold drawn, bar
303 Stainless Steel, Cold worked wire

MQ303H / 12663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.