MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-6 (UNS S20153)
Categories: Metal; Ferrous Metal; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainless such as type 301 or type 304 in many applications based upon technical equivalency and economic considerations. AL 201LN alloy is a natural choice for use at temperatures down to -320°F. The alloy is suited for many ambient temperature structural applications, such as railroad freight cars, truck trailers, coal handling and other bulk transport equipment where there is need for a good combination of corrosion resistance, strength, toughness and ease of fabrication.

Information provided by Allegheny Ludlum Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.857 g/cc0.2839 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 685 MPa
@Temperature 70.0 °C
99400 psi
@Temperature 158 °F
transverse
Tensile Strength, Yield 320 MPa
@Temperature 70.0 °C
46400 psi
@Temperature 158 °F
transverse
Elongation at Break 56 %
@Temperature 70.0 °C
56 %
@Temperature 158 °F
transverse
Izod Impact 208 J153 ft-lbtransverse
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 16 - 17.5 %16 - 17.5 %
Copper, Cu <= 1.0 %<= 1.0 %
Iron, Fe 71 %71 %as balance
Manganese, Mn 6.4 - 7.5 %6.4 - 7.5 %
Nickel, Ni 4.0 - 5.0 %4.0 - 5.0 %
Nitrogen, N 0.10 - 0.25 %0.10 - 0.25 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 201LN Austenitic Stainless steel
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 10% cold reduction
AK Steel 201 Austenitic Stainless steel
302 Stainless Steel, 20% cold reduction
AISI Type S20910 Stainless Steel, 6.4 mm diameter rod, annealed at 1120°C, 30% cold reduction

NL20L0 / 17824

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.