MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical HF380G ABS, High Flow
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Feature: Injection Molding, High Flow

Application: Electric & Electronic Products)

CAS No. 9003-56-9

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 53 g/10 min
@Load 10.0 kg,
Temperature 220 °C
53 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Yield 43.1 MPa
@Thickness 3.20 mm
6260 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 30 %
@Thickness 3.20 mm
30 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Tensile Modulus 2.15 GPa
@Thickness 3.20 mm
311 ksi
@Thickness 0.126 in
1 mm/min; ASTM D638
Flexural Yield Strength 70.6 MPa
@Thickness 3.20 mm
10200 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.40 GPa
@Thickness 3.20 mm
348 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  2.45 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
4.59 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 2.65 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
4.96 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  1.18 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
2.20 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 1.18 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
2.20 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm
Dielectric Strength 34.0 kV/mm864 kV/in
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 V400 - 600 VSolution A; IEC 60112
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.50 mm
15 - 30 sec
@Thickness >=0.0591 in
 15 - 30 sec
@Thickness >=3.00 mm
15 - 30 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/min
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi)  85.0 °C
@Thickness 6.40 mm
185 °F
@Thickness 0.252 in
Unannealed; ASTM D648
 88.0 °C
@Thickness 6.40 mm
190 °F
@Thickness 0.252 in
ASTM D648
Vicat Softening Point 93.0 °C
@Load 5.00 kg
199 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  60.0 °C
@Thickness >=1.50 mm
140 °F
@Thickness >=0.0591 in
UL 746B
 60.0 °C
@Thickness >=3.00 mm
140 °F
@Thickness >=0.118 in
Flammability, UL94  HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
 HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 200 °C356 - 392 °FInjection Molding
Middle Barrel Temperature 190 - 210 °C374 - 410 °FInjection Molding
Front Barrel Temperature 200 - 220 °C392 - 428 °FInjection Molding
Nozzle Temperature 200 - 230 °C392 - 446 °FInjection Molding
Melt Temperature 210 - 240 °C410 - 464 °FInjection Molding
Mold Temperature 40.0 - 70.0 °C104 - 158 °FInjection Molding
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HF380NS ABS, High Flow, General Anti-Static
LG Chemical HF380U ABS, High Flow
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
LG Chemical HF350U ABS, High Flow
LG Chemical HG193S ABS, High Flow, Chemical Resistance

PLAY004 / 148012

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.