MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Trelleborg Emerson & Cuming Stycast® E-1030 One-Component Epoxy Low Stress Encapsulant  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes: Emerson & Cuming E-1030 Stycast® One-Component Epoxy Low Stress Encapsulant
Designed for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low temperatures and provide protection from mechanical shock and vibration. Thermally conductive, good chemical resistance. Mix Ratio (by weight) = 100:14 Cure Type: Heat Bonding Type: Epoxy

The Stycast® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.93 g/cc0.0697 lb/in³
Viscosity 12000 cP
@Temperature 25.0 °C
12000 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7979
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.8
@Frequency 1e+6 Hz
5.8
@Frequency 1e+6 Hz
Dielectric Strength 14.8 kV/mm375 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 159 µm/m-°C
@Temperature 20.0 °C
88.3 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.580 W/m-K4.03 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time >= 180 min>= 3.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® Stycast® 933-48 One-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® 906-1 One-Component Epoxy High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® 926-82-1 One-Component Epoxy High Service Temp Encapsulant
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
CoorsTek Epoxy Seal 216 (ES-216) B-staged epoxy lids

PEMERS09 / 35701

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.