MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® A3 GF 15 1 black PA66 GF15 Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: Description: AKROMID® A3 GF 15 1 black is a 15% glass fibre reinforced, heat stabilised polyamide 6.6 with medium stiffness and strength and HB-listed at UL.

Applications: Applications are components and housings mainly in mechanical engineering and in the automotive industry.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Moisture Absorption 2.5 - 2.7 %
@Temperature 70.0 °C
2.5 - 2.7 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Water Absorption at Saturation 6.7 - 7.3 %6.7 - 7.3 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inISO 294-4
Spiral Flow 99.0 cm39.0 inCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 200 MPa29000 psiH961/30; ISO 2039-1
Tensile Strength at Break 140 MPa20300 psi5 [mm/min]; ISO 527-2
Elongation at Break 3.5 %3.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 6.40 GPa928 ksi1 [mm/min]; ISO 527-2
Flexural Strength 200 MPa29000 psi2 [mm/min]; ISO 178
Flexural Modulus 6.10 GPa885 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched  4.30 J/cm²
@Temperature -30.0 °C
20.5 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
18.9 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/2
CTE, linear, Transverse to Flow 111 µm/m-°C
@Temperature 23.0 - 80.0 °C
61.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-1/2
Melting Point 262 °C504 °FDSC, 10K/min; DIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75/A
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 GF 15 1 black PA66 GF15 Conditioned
Akro-Plastic Akromid® B3 (2500) PA 6 Conditioned
BASF Capron® HPN 9315G Impact Modified, 15% Glass-Filled Nylon 6 (Dry)
Envalior Akulon® S223-DK Nylon 66 (European Grade) (Dry)
Eurotec® Tecomid® NA40 NL E PA6.6, unfilled, natural

PAKRO380 / 182967

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.