MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® K605 HDPE Blow Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Resin Type: Ethylene Homopolymer

Characteristics:

  • Good ESCR
  • Exceptional rigidity
  • Excellent melt strength

Applications:

  • Automotive bumper beams

Information provided by Chevron Phillips.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D1505
ESCR 100% Igepal® 30 hour30 hourCondition B; ASTM D1693
 60 hour60 hourCondition A; ASTM D1693
Melt Flow 11 g/10 min11 g/10 minCondition 190/21.6, HLMI; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ASTM D2240
Tensile Strength, Yield 29.0 MPa4210 psi2 in/min, Type IV bar; ASTM D638
Elongation at Break 750 %750 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.65 GPa239 ksiTangent, 16:1 span:depth,0.5in/min; ASTM D790
Tensile Impact Strength 240 kJ/m²114 ft-lb/in²Type S bar; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FMethod A; ASTM D648
Vicat Softening Point 130 °C266 °FLoading 1, Rate A; ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FType A, type 1 specimen; ASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® C514 HDPE Pipe and Corrugated Extrusion Resin
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade

PCHEVD024 / 20638

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.