MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C26800 (Yellow brass), H04 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent cold workability.

Applications: radiator cores and tanks, flashlight shells, lamp fixtures, fasteners, locks, hinges, plumbing accessories, pins, rivets.

Test specimen: flat products - 1mm thickness.

Key Words: ASTM B36, ASTM B587, SAE J461, SAE J463, MIL-W-6712, CDA 268, ISO CuZn33, CEN CW506L, 67/33 brass, ISO CuZn35, 65/35 brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.47 g/cc0.306 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080
Hardness, Rockwell 30T 7070
Tensile Strength, Ultimate 510 MPa74000 psi
Tensile Strength, Yield 415 MPa60200 psiIn 50 mm
Elongation at Break 8.0 %8.0 %
Tensile Modulus 103 GPa15000 ksi
 105 GPa15200 ksi
Fatigue Strength 97.0 MPa
@Thickness 1.00 mm,
# of Cycles 1.00e+8
14100 psi
@Thickness 0.0394 in,
# of Cycles 1.00e+8
strip
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 35.0 GPa5080 ksi
Shear Strength 295 MPa42800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000640 ohm-cm
@Temperature 20.0 °C
0.00000640 ohm-cm
@Temperature 68.0 °F
annealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.3 µm/m-°C
@Temperature 20.0 - 300 °C
11.3 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 116 W/m-K805 BTU-in/hr-ft²-°F
 116 W/m-K
@Temperature 20.0 °C
805 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 905 - 930 °C1660 - 1710 °F
Solidus 905 °C1660 °F
Liquidus 930 °C1710 °F
Annealing Point 427 - 704 °C800 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 700 °C797 - 1290 °F
Hot-Working Temperature 700 - 820 °C1290 - 1510 °F
Recrystallization Temperature 290 °C554 °FFor strip cold rolled 50% to 1 mm thickness, 0.035 mm initial grain size
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 64 - 68.5 %64 - 68.5 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.15 %<= 0.15 %
Zinc, Zn 31.3 - 36 %31.3 - 36 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C26800 (Yellow brass), H02 Temper flat products
Copper, UNS C26800 (Yellow brass), H01 Temper flat products
Copper, UNS C26800 (Yellow brass), H10 Temper flat products
Copper, UNS C26800 (Yellow brass), OSO70 Temper flat products
Copper, UNS C26800 (Yellow brass), H08 Temper flat products

MC26800c1 / 11121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.