MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite SUMILITE® PLC-2147 SQ Paper Phenolic
Categories: Polymer; Thermoset; Phenolic

Material Notes: Paper Phenolic Single & Double sided Materials for PCB

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 1.0 %1.0 %E-24/50+D-24/23
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 7.00 GPa1020 ksiTD
 9.00 GPa1310 ksiMD
Flexural Strength 150 MPa21800 psiTD
 160 MPa23200 psiMD
Flexural Modulus 7.00 GPa1020 ksiTD
 9.00 GPa1310 ksiMD
Peel Strength 2.00 kN/m11.4 pli35umCF; A
Film Tensile Strength at Break, MD 110 MPa16000 psi
Film Tensile Strength at Break, TD 90.0 MPa13100 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmA
Surface Resistance 1.00e+12 ohm1.00e+12 ohmLaminate Side
 5.00e+12 ohm5.00e+12 ohmAdhesive Side
Dielectric Constant 4.5
@Frequency 1e+6 Hz
4.5
@Frequency 1e+6 Hz
Dissipation Factor 0.038
@Frequency 1e+6 Hz
0.038
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 432 µm/m-°C240 µin/in-°F10°C/min; Z (a1)
CTE, linear, Transverse to Flow 27.0 µm/m-°C15.0 µin/in-°F10°C/min; X (a1)
 37.8 µm/m-°C21.0 µin/in-°F10°C/min; Y (a1)
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FLaser Flash
Flammability, UL94 V-0V-0Flame Resistance
 
Descriptive Properties
Solder Heat Resistance (sec)30S-260 float

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite SUMILITE® PLC-2147 AQ Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 RF Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 GF Paper Phenolic
Sumitomo Bakelite SUMILITE® PLC-2147 GSSM Paper Phenolic
Sumitomo Bakelite SUMILITE® ELC-4762 Glass Epoxy

PSUMIT110 / 193915

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.