MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Haveg Havaflex T.A.-117 Phenolic, Trowelable Ablative Coating  (discontinued **)
Categories: Polymer; Thermoset; Phenolic; Phenolic, Ablative Coating

Material Notes: A two-component modified phenolic ablative coating and adhesive. This material was developed for the U.S. Navy to protect the decks and launchings systems on ships from the extremely high heats (up to 5000°F) and gas velocities (up to Mach 3.0) present during the launching of a missile.

Key Words: Ametek-Haveg Division; Haveg Phenolic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³
Moisture Absorption at Equilibrium 0.67 %0.67 %96 Hours
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8989
Tensile Strength, Ultimate 4.30 MPa624 psi
Elongation at Break 12.5 %12.5 %
Adhesive Bond Strength 23.0 MPa3340 psiTensile Lap Shear; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.513 W/m-K3.56 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic, Ablative Coating
Haveg Havaflex T.A.-118 Phenolic, Trowelable Ablative Coating
Haveg 41NA Phenolic; Silicate Filled
Haveg 41N Phenolic; Silicate Reinforced Ablative Material
Overview of materials for Melamine-Phenolic Copolymer

PPHH00 / 56221

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.