MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borlink™ LE0520 Polyethylene Compound, Crosslinkable, Semiconductive
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0520 is a Strippable Semi conductive Insulation Shielding for Power Cables. LE0520 is suitable for use in triple extrusion processes. Strip forces in the range of 3-6 kN/m (7-14 lbs/half inch) have been found on cables from steam or dry cure vulcanization lines. Stripping of LE0520 from the surface of the insulation is readily initiated and it continues easily over a wide range of temperatures without tearing. it leaves a clean insulation surface. Specifications ICEA S-94-649; ICEA S-97-682; BS 6622; NF C33-223; UTE C 33-223; NF C33-226; and AEIC CS8-07.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 14.4 MPa>= 2090 psiASTM D638
 16.0 MPa2320 psiASTM D638
Elongation at Break 200 %200 %after aging 7 days @ 136°C; ASTM D638
 250 %250 %after aging 42 days @ 100°C
Tensile Set 0.00 %
@Temperature 200 °C
0.00 %
@Temperature 392 °F
Permanent Deformation at 0.2 MPa after 25% elongation under load; IEC 60811-2-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  80 ohm-cm
@Temperature 23.0 °C
80 ohm-cm
@Temperature 73.4 °F
ASTM D991
 400 ohm-cm
@Temperature 90.0 °C
400 ohm-cm
@Temperature 194 °F
ASTM D991
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 280 °C536 °Fmaximum surface temperature, curing tube
Zone 1 90.0 °C194 °F
Zone 2 100 °C212 °F
Zone 3 115 °C239 °F
Zone 4 120 °C248 °F
Die Temperature 120 °C248 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis FL5580 High Density Polyethylene
Borealis Borlink™ LE0594 Crosslinkable Semiconductive Compound for Shielding of Power Cables
Borealis Borlink™ LE0310-99 Polyethylene Thermoplastic Semiconductive Compound
Borealis Borlink™ LE0516 Polyethylene Compound, Crosslinkable, Semiconductive
Borealis Borlink™ LE0595 Crosslinkable Semiconductive Compound for Shielding of Power Cables

PBOREA509 / 108768

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.