MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-socket connectors, power switches), halogen- and antimony free.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Linear Mold Shrinkage, Flow 0.0055 cm/cm0.0055 in/in60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0147 cm/cm0.0147 in/in60x60x2 mm; ISO 294
Melt Flow 32.2 g/10 min
@Load 2.16 kg,
Temperature 275 °C
32.2 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 105 MPa15200 psi50 mm/min; ISO 527-2
Elongation at Break 2.4 %2.4 %50mm/min; ISO 527-2
Modulus of Elasticity 9.50 GPa1380 ksiISO 527-2
Flexural Strength 180 MPa26100 psiISO 178
Charpy Impact Unnotched 4.20 J/cm²20.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 93
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohmIEC 93
Dielectric Constant 3.63.6IEC 250
Dissipation Factor 0.01420.0142IEC 250
Comparative Tracking Index 600 V600 VTest solution A; IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 - 120 µm/m-°C
@Temperature 23.0 - 80.0 °C
16.7 - 66.7 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 53752
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 201 °C394 °FISO 75-2
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °FInjection-molding
Mold Temperature 60.0 - 100 °C140 - 212 °F
 
Descriptive Properties
ColorNatural, Colored, Black and Special Colors
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT
LG Chemical AF342F ABS, Flame Retardant, High Flow
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned)
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry)

PBASG0114 / 131748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.