MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%
Stress Relaxation after 1000 hrs @ 200°C: 69%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 5
Formability Ratio (bad Way): 10
Superficial Hardness: 30N 53-62

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-194
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 33 - 4233 - 42
Hardness, Vickers 325 - 413325 - 413
Tensile Strength, Ultimate 1200 - 1320 MPa174000 - 191000 psi
Tensile Strength, Yield 1030 - 1250 MPa149000 - 181000 psi
Elongation at Break 3.0 - 12 %3.0 - 12 %
Modulus of Elasticity 131 GPa19000 ksi
Fatigue Strength 340 - 410 MPa
@# of Cycles 1.00e+8
49300 - 59500 psi
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000610 - 0.0000101 ohm-cm0.00000610 - 0.0000101 ohm-cm17-28% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C1600 - 1800 °F
Solidus 870 °C1600 °F
Liquidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.8 - 2.0 %1.8 - 2.0 %
Co + Ni >= 0.20 %>= 0.20 %
Co + Ni + Fe <= 0.60 %<= 0.60 %
Copper, Cu 98 %98 %as balance
Lead, Pb <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200)
Ampco Metal AMPCOLOY® 83 Beryllium Copper, Extrusion
Ampco Metal AMPCOLOY® 88 Beryllium Copper, Extrusion
Ampco Metal AMPCOLOY® 89 Beryllium Copper, Extrusion
Ampco Metal AMPCOLOY® 91 Beryllium Copper, Extrusion <35mm

NBB498 / 15199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.