MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walled corrugated pipes and profiles.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psi50mm/min; ISO 527-2
Elongation at Yield 10 %10 %50mm/min; ISO 527-2
Flexural Modulus 1.10 GPa160 ksi2mm/min; ISO 178
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 200 - 220 °C392 - 428 °F
Die Temperature 210 - 220 °C410 - 428 °F
Melt Temperature 210 - 230 °C410 - 446 °F
Head Temperature 210 - 220 °C410 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 1640 Polypropylene, Heterophasic Copolymer, Non-pressure Pipes
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes
Borealis BA11CF Polypropylene Copolymer
Ineos T00G-00 Polypropylene Impact Copolymer
Ineos N01G-02 Polypropylene Impact Copolymer

PBOREA303 / 108563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.