MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Röchling Polystone® P MG Medical Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes:

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792
Water Absorption <= 0.10 %<= 0.10 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ASTM D2240
Tensile Strength, Yield 32.4 MPa4700 psiASTM D638
Elongation at Break >= 400 %>= 400 %ASTM D638
Flexural Modulus 1.24 GPa180 ksiASTM D790
Izod Impact, Notched 0.534 J/cm1.00 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.25 - 0.280.25 - 0.28
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 108 µm/m-°C60.0 µin/in-°FASTM D696
Melting Point 162 °C323 °F
Maximum Service Temperature, Air 82.2 °C180 °F
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
USP Class VI YesYes
 
Descriptive Properties
ColorWhite, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPM H350 Polypropylene, Homopolymer Medical Grade
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
Röchling SUSTAPEI® MG PEI/Medical Grade
Total PPR 7425 Polypropylene, Injection Molding Grade
Total PPM R021 Polypropylene, Random Copolymer for Medical Grade

PROCH9024 / 232727

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.