MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldability and outstanding surface appearance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.74 g/cc0.0629 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 207 MPa30000 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 245 MPa35500 psi5mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5mm/min; ISO 527
 3.0 %3.0 %0.2 in/min; ASTM Test
Tensile Modulus 22.4 GPa3250 ksi1mm/min; ISO 527
Flexural Strength 355 MPa51500 psiISO Data
 378 MPa54800 psiASTM Test
Flexural Modulus 17.3 GPa2510 ksiASTM Test
 18.0 GPa2610 ksiISO Data
Izod Impact, Notched 1.55 J/cm
@Thickness 3.17 mm
2.90 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Unnotched 13.88 J/cm26.00 ft-lb/inASTM Test
Izod Impact, Notched (ISO) 12.5 kJ/m²5.95 ft-lb/in²ISO Test
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FASTM Test
 214 °C417 °FISO 75
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
ColorBK-102
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NAX0 GR70 NL HS PA6.6, 70% glass fiber reinforced, heat stabilized, natural
Aluminum A380.0-F Die Casting Alloy
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Conditioned)

PBASF9371 / 85135

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.