MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Colorite Polymers 2007F Rigid PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the production of medical devices that require gamma or ETO sterilization (and can also be formulated to withstand the degradation and discoloration associated with ETO sterilization). These compounds are noted for their low odor and good early color characteristics. Custom color matching is also available. Manufacturer's Rigid PVC compounds offer good heat stability and high-flow characteristics for ease of processing. They are formulated to meet USP class VI approval. Complete traceability and lot identification of all compounds are maintained in our ISO 9002 manufacturing facility.

Information provided by Colorite Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7676ASTM D2240
Tensile Strength, Ultimate 45.5 MPa6600 psiASTM D638
Izod Impact, Notched 11.7 J/cm22.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C162 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Color/ClarityClear Blue Tint
End UsesFDA, Sheet, Bottles
Process Type Extrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 2010 Rigid PVC
Colorite Polymers 2007 Rigid PVC
Colorite Polymers 2007UV Rigid PVC
Colorite Polymers 2019F Rigid PVC
Colorite Polymers 2002 Rigid PVC

PCOL082 / 28801

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.