MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior properties, along with excellent drawability, make this a versatile resin for both monolayer and multiplayer packaging and cast stretch film.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Bag in Box
  • Barrier Food Packaging
  • Blown Film
  • Cast Film
  • Cast Stretch Film
  • Diaper Backsheet
  • Form Fill and Seal Packaging
  • Hygiene Film
  • Packaging Films
  • Personal Care

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ExxonMobil method
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.27 MPa1200 psiASTM D882
Film Tensile Strength at Yield, TD 7.58 MPa1100 psiASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 730 %730 %ASTM D882
Puncture Energy 4.41 J3.25 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 150 g150 gASTM D1922
Elmendorf Tear Strength TD 460 g460 gASTM D1922
Dart Drop Test 140 g0.309 lbASTM D1709
Film Tensile Strength at Break, MD 66.9 MPa9700 psiASTM D882
Film Tensile Strength at Break, TD 48.3 MPa7000 psiASTM D882
1% Secant Modulus, MD 103 MPa15000 psiASTM D882
1% Secant Modulus, TD 124 MPa18000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 114 °C<= 237 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 2.2 %2.2 %ASTM D1003
Gloss 87 %87 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force11 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polypropylene Spelling Note
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade)
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications
ExxonMobil Enable™ 40-02HH Metallocene Polyethylene Resin

PEX99057 / 175293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.