MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC
Categories: Ceramic; Carbide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.68 g/cc0.0968 lb/in³
Porosity 14 %14 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.051012 GPa
@Temperature 250 °C
7.3988 ksi
@Temperature 482 °F
 0.051012 GPa
@Temperature 1400 °C
7.3988 ksi
@Temperature 2550 °F
Compressive Strength 206 MPa29900 psiCold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.30 µm/m-°C
@Temperature 1000 °C
2.39 µin/in-°F
@Temperature 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 0.30 %0.30 %
SiC 95 %95 %
 
Descriptive Properties
Refractories Under Load(2kg/cm²,T2°C)1,700<

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories SSB-1 Bricks, Reaction Bonded SiC
Chosun Refractories SBN-1 Bricks, Reaction Bonded SiC
China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
Skamol Group SUPER 1100 ET Calcium Silicate Insulating Slab
Thermal Ceramics Kaocrete 249 C Low Cement Castables

CCHOS049 / 123993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.