MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Terluran® HI-12 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.
  • Very high toughness
  • Easy flowing
  • UL 94 HB (1.6 & 3.2 mm)

    Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.21 %
@Temperature 23.0 °C
0.21 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation 1.03 %
@Temperature 23.0 °C
1.03 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 14 g/10 min
@Load 10.0 kg,
Temperature 220 °C
14 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 101101IEC 2039-2
Ball Indentation Hardness 80.0 MPa11600 psiISO 2039-1
Tensile Strength, Yield 40.0 MPa5800 psiISO 527
Elongation at Yield 2.7 %2.7 %ISO 527
Tensile Modulus 1.90 GPa276 ksiISO 527
Flexural Strength 58.0 MPa8410 psiISO 178
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 31.0 kJ/m²
@Temperature 23.0 °C
14.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
 35.0 kJ/m²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ASTM D 256
Charpy Impact Unnotched  16.0 J/cm²
@Temperature -30.0 °C
76.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0054
@Frequency 100 Hz
0.0054
@Frequency 100 Hz
IEC 60250
 0.0082
@Frequency 1e+6 Hz
0.0082
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 110 µm/m-°C44.4 - 61.1 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 80.0 °C176 °F
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FISO 75
Vicat Softening Point  96.0 °C
@Load 5.10 kg
205 °F
@Load 11.2 lb
50°C/h; ISO 306
 104 °C
@Load 1.02 kg
219 °F
@Load 2.25 lb
50°C/h; ISO 306
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °FISO 294
Mold Temperature 40.0 - 60.0 °C104 - 140 °FISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-747 ABS
INEOS Styrolution Terluran® HI-10 ABS
Chi Mei Polylac® PA-757 ABS
INEOS Styrolution Terluran® GP-22 ABS
LG Chemical HI-121 ABS, High Impact

PBASF9053A / 159692

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.