MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen PP HP1886 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Hostalen PP HP1886 is a very low flow random copolymer with good stiffness/toughness balance, outstanding creep and stress cracking resistance. Hostalen PP HP1886 features low haze and yellowing resistance in contact with cooling water. Typical customer use is automotive expansion tanks. Hostalen PP HP1886 is not intended for medical and pharmaceutical applications. Applications: Non-fuel Reservoirs, Under hood

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 0.90 g/10 min0.90 g/10 minISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 36.0 MPa5220 psi50mm/min; ISO 527-1,-2
Elongation at Yield 10.3 %10.3 %50mm/min; ISO 527-1,-2
Tensile Modulus 1.40 GPa203 ksi1% secant; ISO 527-1,-2
Charpy Impact Unnotched NBNBType 1, edgewise, Notch A; ISO 179
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °Funannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °Funannealed; ISO 75A-1,-2
Vicat Softening Point 151 °C304 °FA50; ISO 306
 
Descriptive Properties
Processing Methodinjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom PP HH42L 356015 Polypropylene
LyondellBasell Hostalen PP H2142 12 Polypropylene Copolymer
LyondellBasell Hostalen PP H2493 Polypropylene Copolymer
LyondellBasell Hostalen PP H1850 Polypropylene Copolymer
LyondellBasell Hostalen PP H4122 103220 Polypropylene Copolymer

PEQT8519 / 220154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.