MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.

Information provided by Honeywell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D1505
Density 1.22 g/cc0.0440 lb/in³Yield Density
Water Vapor Transmission  0.0780 g/m²/day
@Temperature 25.0 °C
0.00502 g/100 in²/day
@Temperature 77.0 °F
60%RH; ASTM F1249
 0.155 g/m²/day
@Temperature 30.0 °C
0.00998 g/100 in²/day
@Temperature 86.0 °F
60%RH; ASTM F1249
 0.510 g/m²/day
@Temperature 40.0 °C
0.0328 g/100 in²/day
@Temperature 104 °F
75%RH; ASTM F1249
 0.780 g/m²/day
@Temperature 37.8 °C
0.0502 g/100 in²/day
@Temperature 100 °F
100%RH; ASTM F1249
Oxygen Transmission Rate 202 - 233 cc/m²/day13.0 - 15.0 cc/100 in²/day25°C / 0%RH; ASTM D3985
Thickness 33.0 microns1.30 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 17.9 - 20.0 MPa2600 - 2900 psiASTM D882
Film Tensile Strength at Yield, TD 17.9 - 20.0 MPa2600 - 2900 psiASTM D882
Film Elongation at Break, MD 75 - 100 %75 - 100 %ASTM D882
Film Elongation at Break, TD 225 - 325 %225 - 325 %ASTM D882
Film Elongation at Yield, MD 7.0 - 9.0 %7.0 - 9.0 %ASTM D882
Film Elongation at Yield, TD 7.0 - 9.0 %7.0 - 9.0 %ASTM D882
Secant Modulus, MD 0.448 - 0.586 GPa65.0 - 85.0 ksiASTM D882
Secant Modulus, TD 0.448 - 0.586 GPa65.0 - 85.0 ksiASTM D882
Falling Dart Impact 0.813 - 1.08 J0.600 - 0.800 ft-lbASTM D4272
Coefficient of Friction 0.40 - 0.600.40 - 0.60Aclar® to metal; ASTM D1894
Coefficient of Friction, Static 0.60 - 0.800.60 - 0.80Aclar® to metal; ASTM D1894
Tear Strength Test 350 - 375350 - 375graves tear MD, grams/mil; ASTM D1004
 350 - 375350 - 375graves tear TD, grams/mil; ASTM D1004
Film Tensile Strength at Break, MD 26.2 - 31.7 MPa3800 - 4600 psiASTM D882
Film Tensile Strength at Break, TD 17.9 - 20.0 MPa2600 - 2900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 2.0 - 3.0 %2.0 - 3.0 %ASTM D1003
Gloss 130 - 140 %130 - 140 %at 20°; ASTM D523
 
Descriptive Properties
Interlayer Bond Strengthmin 450 g/inASTM F904
Puncture Strength250-300 gASTM F1309

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger XP-46 Compression Molded Unfilled PCTFE
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film
Daikin NEOFLON® M-300P PCTFE
Honeywell ACLAR® Cx™ 8A Heat Sealable, Co-Extruded CTFE Film

PALA38 / 23130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.