MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

304 Stainless Steel (UNS S30400); Annealed Strip
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic Cr-Ni stainless steel. Better corrosion resistance than Type 302. High ductility, excellent drawing, forming, and spinning properties. Essentially non-magnetic, becomes slightly magnetic when cold worked. Low carbon content means less carbide precipitation in the heat-affected zone during welding and a lower susceptibility to intergranular corrosion.

Applications: beer kegs, bellows, chemical equipment, coal hopper linings, cooking equipment, cooling coils, cryogenic vessels, dairy equipment, evaporators, flatware utensils, feedwater tubing, flexible metal hose, food processing equipment, hospital surgical equipment, hypodermic needles, kitchen sinks, marine equipment and fasteners, nuclear vessels, oil well filter screens, refrigeration equipment, paper industry, pots and pans, pressure vessels, sanitary fittings, valves, shipping drums, spinning, still tubes, textile dyeing equipment, tubing.

Corrosion Resistance: resists most oxidizing acids and salt spray.

UNS S30400; AMS 5501, 5513, 5560, 5565; ASME SA182, SA194 (8), SA213, SA240; ASTM A167, A182, A193, A194

Key Words: aisi304, AISI 304, T304, T 304, SUS304, SS304, 304SS, 304 SS, UNS S30400, AMS 5501, AMS 5513, AMS 5560, AMS 5565, AMS 5566, AMS 5567, AMS 5639, AMS 5697, ASME SA182, ASME SA194 (8), ASME SA213, ASME SA240, ASME SA249, ASME SA312, ASME SA320 (B8), ASME SA358, ASME SA376, ASME SA403, ASME SA409, ASME SA430, ASME SA479, ASME SA688, ASTM A167, ASTM A182, ASTM A193, ASTM A194, ASTM A666, FED QQ-S-763, MILSPEC MIL-S-5059, SAE 30304, DIN 1.4301, X5CrNi189, B.S. 304 S 15, EN 58E, PN 86020 (Poland), OH18N9, ISO 4954 X5CrNi189E, ISO 683/13 11, 18-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B <= 92<= 92
 <= 92<= 92
Tensile Strength, Ultimate >= 515 MPa>= 74700 psi
 >= 515 MPa>= 74700 psi
Tensile Strength, Yield  >= 205 MPa
@Strain 0.2 %
>= 29700 psi
@Strain 0.2 %
 >= 205 MPa
@Strain 0.2 %
>= 29700 psi
@Strain 0.2 %
Elongation at Break >= 40 %>= 40 %
 >= 40 %>= 40 %
Modulus of Elasticity 193 GPa28000 ksi
Poissons Ratio 0.290.29
Shear Modulus 77.0 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000720 ohm-cm
@Temperature 20.0 °C
0.0000720 ohm-cm
@Temperature 68.0 °F
 0.000116 ohm-cm
@Temperature 650 °C
0.000116 ohm-cm
@Temperature 1200 °F
Magnetic Permeability 1.0201.020at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
9.89 µin/in-°F
@Temperature 32.0 - 599 °F
 18.4 µm/m-°C
@Temperature 0.000 - 538 °C
10.2 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.2 W/m-K
@Temperature 0.000 - 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 32.0 - 212 °F
 21.5 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 66.345 - 74 %66.345 - 74 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 10.5 %8.0 - 10.5 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %
 
Descriptive Properties
SpecificationASTM A 167

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
302 Stainless Steel, annealed strip
AISI 303 Cast Stainless Steel, ASTM A582
304 Stainless Steel (UNS S30400); 1/4 Hard Bar, Plate, Sheet, and Strip
410 Stainless Steel
304 Stainless Steel (UNS S30400); 1/2 Hard Bar, Plate, Sheet, and Strip

MQ304A15 / 151037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.