MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Prodways PLASTCure ABS 3650 3D Printing Polymer  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: High transparency. Good chemical resistance. Fast and adaptable material to a wide range of building conditions. Suited for tetrashell and foundry applications on large parts

Applications: Highly suitable for investment casting of industrial elements like impellers or aeronautical parts, even in Titanium or high level alloys

Information provided by Genistar.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³
Water Absorption 1.2 - 1.4 %1.2 - 1.4 %ASTM D570
Viscosity 100 - 300 cP
@Temperature 23.0 °C
100 - 300 cP
@Temperature 73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85
Tensile Strength at Break 50.0 - 60.0 MPa7250 - 8700 psiASTM D638
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %ASTM D638
Tensile Modulus 2.40 - 2.70 GPa348 - 392 ksiASTM D638
Flexural Strength 85.0 - 95.0 MPa12300 - 13800 psiASTM D790-10
Flexural Modulus 1.80 - 2.20 GPa261 - 319 ksiASTM D790-10
Flexural Strain at Break 10 - 12 %10 - 12 %ASTM D790-10
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 - 71.0 °C153 - 160 °FISO 75-2
 
Descriptive Properties
AppearanceClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Eastman Tritan™ EX401 Copolyester
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polylactic Acid (PLA) Biopolymer

PPRODW908 / 172314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.