MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alliance S-28B Samarium Cobalt Magnetic Material  (discontinued **)
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Cobalt Alloy

Key Words: SmCo Magnet Magnets
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.40 g/cc0.303 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 640640
Modulus of Elasticity 150 GPa21800 ksi
Flexural Strength 90.0 - 150 MPa13100 - 21800 psi
Compressive Strength 650 MPa94300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000750 - 0.0000850 ohm-cm0.0000750 - 0.0000850 ohm-cm
Magnetic Coercive Force, Hc 10000 Oe10000 Oe
 20000 Oe20000 OeIntrinsic
Magnetic Remanence, Br 10900 Gauss10900 Gauss
Magnetic Maximum Energy Product, BH 28 MGOe28 MGOe
Curie Temperature 750 °C1380 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 µm/m-°C
@Temperature 20.0 °C
5.56 µin/in-°F
@Temperature 68.0 °F
Parallel DOM
CTE, linear, Transverse to Flow 12.0 µm/m-°C
@Temperature 23.0 °C
6.67 µin/in-°F
@Temperature 73.4 °F
Perpendicular to M
Specific Heat Capacity 0.390 J/g-°C0.0932 BTU/lb-°F
Thermal Conductivity 12.0 W/m-K83.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 300 °C572 °F
 
Descriptive Properties
Reversible Temp Coef., Bd-0.03 %/°C
Reversible Temp Coef., Hd+0.23 %/°C
Temperature Coefficient, Br-0.03 %/°C(20-100°C)
Temperature Coefficient, Hci-0.18 %/°C(20-100°C)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance S-30A Samarium Cobalt Magnetic Material
Alliance S-22B Samarium Cobalt Magnetic Material
Alliance A-5-7 Alnico Magnetic Material
Alliance A-6 Alnico Magnetic Material
Alliance N-30EH Neodymium Iron Boron Magnetic Material

NALLIAN59 / 14884

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.